Radici Radilon® A RV150 (cond.) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® A RV150 (cond.) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
(Dry)
Water Absorption 7.9 %
7.9 %
initially dry
Moisture Absorption at Equilibrium 2.3 %
2.3 %
initially dry
Viscosity Measurement 145
145
cm³/g Viscosity Number
Mechanical Properties Metric English Comments
Tensile Strength, Yield 85.0 MPa
12300 psi
Elongation at Break 13 %
13 %
Nominal
Elongation at Yield 4.9 %
4.9 %
Tensile Modulus 3.90 GPa
566 ksi
Charpy Impact Unnotched 3.70 J/cm²

@Temperature -30.0 °C
17.6 ft-lb/in²

@Temperature -22.0 °F
7.50 J/cm²

@Temperature 23.0 °C
35.7 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.590 J/cm²

@Temperature -30.0 °C
2.81 ft-lb/in²

@Temperature -22.0 °F
0.850 J/cm²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
(Dry)
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 550 V
550 V