Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 0.850 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Polykemi AB SCANMID 6 B12^ F50 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
Radici Radiflam® A RV300AF (cond.) Nylon 66-30GF
Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g..
Charpy Impact, Notched 0.850 J/cm²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® A RV150 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® S RV200 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact, Notched 0.850 J/cm²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® S RCP3010LK (cond.) Nylon 6
PA6 30% Glass Fiber and mineral filler reinforced injection molding grade. Good stiffness and good dimensional stability. Heat stabilized, good surface finish.Information provided by Radici group.
Charpy Impact, Notched 0.850 J/cm²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® S RCV3015 (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact, Notched 0.850 J/cm²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Charpy Impact, Notched 0.850 J/cm²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Borealis BD950MO Polypropylene Copolymer
BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability..
Charpy Impact, Notched 0.850 J/cm²

@Temperature -20.0 °C
4.04 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis EE002AE Polypropylene Elastomer Modified
EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties..
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Polyram RamSter PF305G6 PBT, 30% Glass Fiber
30% Glass fiber reinforced, PBT for injection molding applications.Information provided by Polyram.
Charpy Impact, Notched 0.850 J/cm²

@Temperature -20.0 °C
4.04 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Total PPC 7810 Polypropylene, Heterophasic Copolymer, High Impact
Polypropylene PPC 7810 is a very high impact heterophasic copolymer with a Melt Flow index of 15 g/10 min.Polypropylene PPC 7810 has been specially developed for high impact and heavy duty applicati..
Charpy Impact, Notched 0.850 J/cm²

@Temperature -20.0 °C
4.05 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Unipetrol PP MONSTEN® EB 501 Polypropylene Impact Copolymer
Made for extrusion applications. LHTA stabilization. Impact copolymer.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
BASF Ultraform® N2640 E4 POM
Description: Is a POM + MBS, elastomer-modified injection-molding grade with high toughness and high weld line strength.Information provided by BASF
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Dry)
Description: Ultramid B3WG6 CR BK23210 s a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade for crash relevant applications.Information provided by BASF
Charpy Impact, Notched 0.850 J/cm²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® A CF350 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® A RV330 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® A RV350 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Rynite® 530 BK503 PET  (Unverified Data**)
Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, ..
Charpy Impact, Notched 0.850 J/cm²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
BASF Ultraform® N2644 Z9 POM + PUR
Description: Elastomer modified injection molding grade for applications requiring low modulus. Good acoustic damping.Information provided by BASF
Copyright © lookpolymers.com All Rights Reserved