Material Notes:
Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. High acrylonitrile (ACN) content = 40% plus. Copolymer of acrylonitrile and butadiene.Applications: The high acrylonitrile content of this compound increases resistance to petroleum-based oils and fuels. Suitable for use in Aerospace applications.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
55 - 85
55 - 85
°IRHD, ±15 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 5.25 MPa
761 psi
-25% change after 70 hours @ 100°C; ASTM D412
7.00 MPa
1020 psi
ASTM D412
Elongation at Break 225 %
225 %
-25% change after 70 hours @ 100°C; ASTM D412
300 %
300 %
ASTM D412
Compression Set 25 %
25 %
24 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Non-brittle after 3 minutes
-35.0 °C
-31.0 °F
Flash Point >= 300 °C
>= 572 °F