Polymer Property : Tensile Strength, Yield = 761 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.25 MPa
761 psi
ASTM D412
Polymax® Maxelast® F02-087A TPE, Halogen Free Extrusion Grade
Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to..
Tensile Strength, Yield 5.25 MPa
761 psi
-25% change after 70 hours @ 125°C; ASTM D412
Precision Polymer Engineering H80B Epichlorohydrin
Peroxide Cured, Epichlorohydrin Rubber, 75-85 °IRHD. Terpolymer of epichlorohydrin, ethylene oxide and an unsaturated monomer. To ASTM D2000 line call-out: M3CH608, A25, B14, EO16, EO36, F17. AS..
Tensile Strength, Yield 5.25 MPa
761 psi
-25% change after 70 hours @ 100°C; ASTM D412
Precision Polymer Engineering N65H Nitrile Rubber
Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. High acrylonitrile (ACN) content = 40% plus. Copolymer of acrylonitrile and butadiene.Applications: The high acrylonitrile content of this compound inc..
Tensile Strength, Yield 5.25 MPa
761 psi
ASTM D412
Precision Polymer Engineering S60S Silicone Rubber
Red Silicone Rubber, 56-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Excellent steam resistance. Formulated using only those ingredients determi..
Tensile Strength, Yield 5.25 MPa
761 psi
-25% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering V75V Fluoroelastomer Compound
Special steam resistant, Fluoroelastomer Rubber, 70-80 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out MHK707, A1-10, B37, E..