Material Notes:
UV stabilized acetal copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
DIN 53479
Linear Mold Shrinkage 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
ASTM-D638
Elongation at Break 30 %
30 %
ASTM-D638
Tensile Modulus 2.00 GPa
290 ksi
ASTM-D790
Flexural Strength 75.0 MPa
10900 psi
ASTM-D790
Flexural Modulus 2.50 GPa
363 ksi
ASTM-D790
Izod Impact, Notched 0.600 J/cm

@Temperature 23.0 °C
1.12 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
DIN 53461
Vicat Softening Point 150 °C
302 °F
ASTM-D1525
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in