Karina E 605D06/476-AT Blue PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 605D06/476-AT Blue PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.17 - 1.23 g/cc
1.17 - 1.23 g/cc
ASTM D 792
ASTM Color -24.28 - -21.28
-24.28 - -21.28
Color A, ME 12
-13.75 - -10.75
-13.75 - -10.75
Color B, ME 12
75.63 - 78.63
75.63 - 78.63
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 62

@Time 15.0 sec
58 - 62

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 6.86 MPa
>= 996 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Injection Molded Parts