Material Notes:
UV stabilized PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
DIN 53479
Moisture Absorption at Equilibrium 8.0 %
8.0 %
DIN 53714
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM-D638
Elongation at Break 45 %
45 %
ASTM-D638
Flexural Strength 80.0 MPa
11600 psi
ASTM-D790
Flexural Modulus 2.20 GPa
319 ksi
ASTM-D790
Izod Impact, Notched 5.00 J/cm

@Temperature 23.0 °C
9.37 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
DIN 53461
Vicat Softening Point 120 °C
248 °F
ASTM-D1525
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
DIN 53482
Dielectric Strength 24.0 kV/mm
610 kV/in
VDE 0303/4