Material Notes:
A chemically coupled 20% long glass fibers reinforced black polypropylene, heat stabilized for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
ISO 527
Elongation at Break 2.0 %
2.0 %
ISO 527
Tensile Modulus 5.00 GPa
725 ksi
ISO 527
Flexural Strength 130 MPa
18900 psi
ISO 178
Flexural Modulus 4.10 GPa
595 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
ISO 180
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 149 °C
300 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Flame Spread 10 mm/min
0.39 in/min
FMVSS302