Material Notes:
Polyamide 66 filled with PTFE to improve wear resistance in molded partsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
DIN 53479
Water Absorption 8.5 %
8.5 %
DIN 53495
Moisture Absorption at Equilibrium 2.8 %
2.8 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
ASTM-D638
Elongation at Break 15 %
15 %
ASTM-D638
Tensile Modulus 2.50 GPa
363 ksi
ASTM-D790
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
ASTM-D790
Izod Impact, Notched 0.650 J/cm

@Temperature 23.0 °C
1.22 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Users viewing this material also viewed the following: