Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® MQ 70 High Density Polyethylene - Injection Molding Eraclene MQ 70 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MQ 70 is suggested in applications for which high creep, impact and .. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® MQ 74 High Density Polyethylene - Injection Molding Eraclene MQ 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. This resin is suggested in applications for which high creep, impact and st.. |
|||
Izod Impact, Notched | 0.650 - 0.800 J/cm | 1.22 - 1.50 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LAPEX A G/20 20% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM Data |
Dow Questra® EA503 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LAESTRA G/30-V0CT1 30% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® BR111BL is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical proper.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
LG Chemical LUCEL N115-LD Anti Mold Deposit POM, Unreinforced, Internally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMAX GP-5106F General Purpose PBT, 10% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMAX HF-5306F High Flow PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0320 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 0.650 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.22 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PBT-R0N Flame Retardant PBT Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation .. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-1935 HS Polyphthalamide (PPA), 35% Glass Fiber Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East) VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP SH1100A PA12 LNP* Thermocomp* SH1100A is a Nylon 12, High Specificy Gravity compound containing proprietary fillers. |
|||
Izod Impact, Notched | 0.650 J/cm @Thickness 3.20 mm |
1.22 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 515 Flame Retardant Polystyrene Characteristics Good flow properties Good balance of toughness and rigidity Available in any colorProcessing Injection molding Extrusion Applications Electrical switch boards MCB distribution bo.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Asia Pacific) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 J/cm @Thickness 3.17 mm |
1.22 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika C300VN Characteristics: Flame resistant, transparent (flame resistance: UL94 V0, 0.8 mm) High flowInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -20.0 °C |
1.22 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Total PPC 4624WZ Polypropylene, Impact Copolymer ATOFINA 4624WZ polypropylene is a nucleated impact copolymer, combining good fluidity and mechanical properties. 4624WZ is characterized by significantly improved resistance, while maintaining exce.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM-D256 |
Braskem GD5150K HDPE High Density Extrusion Polyethylene GD5150K is a high-density polyethylene specially developed for the manufacturing of insulation for wires and cables demanding high extrusion velocity. It has medium molar mass, shows good dielectric.. |
|||
Izod Impact, Notched | 0.650 J/cm @Thickness 3.17 mm |
1.22 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Petra® 110 BK-112 15% Glass Filled PET Petra 110 is a 15% glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a good combination of performance properties including good strength a.. |
|||
Izod Impact, Notched | 0.650 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
1.22 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
Notched V 10 mm; ASTM D256 |
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **) Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ISO 180 |
Solvay Specialty Polymers Primef® 4002 40% GF PPS, High Fluidity Grade
(discontinued **) Used for injection molding of high performance parts. |
|||
Izod Impact, Notched | 0.650 J/cm @Diameter 3.17 mm, Temperature -20.0 °C |
1.22 ft-lb/in @Diameter 0.125 in, Temperature -4.00 °F |
bar; ASTM D256 |
BP Amoco Acctuf® 3541 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purpose, High melt flowComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded sam.. |
|||
Izod Impact, Notched | 0.650 - 2.94 J/cm | 1.22 - 5.50 ft-lb/in | Average value: 1.21 J/cm Grade Count:19 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |