Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® MQ 70 High Density Polyethylene - Injection Molding Eraclene MQ 70 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MQ 70 is suggested in applications for which high creep, impact and .. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® MQ 74 High Density Polyethylene - Injection Molding Eraclene MQ 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. This resin is suggested in applications for which high creep, impact and st.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARPEEK 10 K/30 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, at 50% RH
(disc AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® MQ 70 U High Density Polyethylene - Injection Molding Eraclene MQ 70 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution and a mediu.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
SABIC PP681K Polypropylene Random Copolymer for Injection Molding Product Description: PP 681K is specially developed for producing injection molded articles with high clarity and also has better impact properties than homo PP counterparts.PP 681K has the followi.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LAPEX A G/20 20% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
LG Chemical LUCEL N115-LD Anti Mold Deposit POM, Unreinforced, Internally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMAX HF-5306F High Flow PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0320 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0320 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
Solvay TECHNYL® C 50 H2 PA6, DRY Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This p.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon DX92440 PC LNP STAT-KON* DX92440 is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp FF004 PE LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL N1150 PPE+PS Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Asia Pacific) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamShine PW300G7 SAN, 35% Glass Fiber 35% glass fiber reinforced SAN for very high rigidity injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM1109 Acetal, General Purpose General purpose polyacetal copolymer for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM3013G4 Acetal, 20% Glass Fiber 20% Glass fiber reinforced polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -20.0 °C |
1.22 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Total PPC 4624WZ Polypropylene, Impact Copolymer ATOFINA 4624WZ polypropylene is a nucleated impact copolymer, combining good fluidity and mechanical properties. 4624WZ is characterized by significantly improved resistance, while maintaining exce.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM-D256 |
Braskem GD5150K HDPE High Density Extrusion Polyethylene GD5150K is a high-density polyethylene specially developed for the manufacturing of insulation for wires and cables demanding high extrusion velocity. It has medium molar mass, shows good dielectric.. |
|||
Izod Impact, Notched | 0.650 J/cm @Thickness 3.17 mm |
1.22 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Petra® 110 BK-112 15% Glass Filled PET Petra 110 is a 15% glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a good combination of performance properties including good strength a.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 J/cm @Diameter 3.17 mm, Temperature -20.0 °C |
1.22 ft-lb/in @Diameter 0.125 in, Temperature -4.00 °F |
bar; ASTM D256 |
BP Amoco Acctuf® 3541 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purpose, High melt flowComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded sam.. |