Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyplastic Armlen® PP MF 15-3 FR Polypropylene Homopolymer, Mineral Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant , Polypropylene, Mineral Reinforced
Manufacturer Polyplastic Group
Trade Name Armlen®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastic Armlen® PP MF 15-3 FR Polypropylene Homopolymer, Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant, RoHS compliantInformation provided by PolyPlastic Group.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
ISO 294
Linear Mold Shrinkage, Transverse 0.0090 - 0.011 cm/cm
0.0090 - 0.011 in/in
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ISO 527
Elongation at Break 25 %
25 %
ISO 527
Flexural Modulus 2.00 GPa
290 ksi
ISO 178
Charpy Impact Unnotched 1.50 J/cm²

@Temperature -40.0 °C
7.14 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eU
6.20 J/cm²

@Temperature 23.0 °C
29.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ISO 75
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Glow Wire Test 960 °C

@Thickness 1.60 mm
1760 °F

@Thickness 0.0630 in
IEC 60695-2-1
Electrical Properties Metric English Comments
Comparative Tracking Index 500 V
500 V
IEC 60112
Processing Properties Metric English Comments
Melt Temperature 220 °C
428 °F
Mold Temperature 60.0 °C
140 °F
Users viewing this material also viewed the following: