Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 96 FRD 1 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 Y 35 FRY 7 PA66, 35% mineral filling FeaturesPA 66 for injection moulding, chemically reinforced with 35 % mineral filler and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 /3.2 mm/ in accordance wi.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -40.0 °C |
7.14 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eU |
Polyplastic Armlen® PP MF 15-3 FR Polypropylene Homopolymer, Mineral Filled Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 51 T 30 Polypropylene Copolymer, 30% Micronized Talc FeaturesModified copolymer PP for injection moulding with the content of 30% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden f.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 56 T FRD 1 PP, flame retardant FeaturesModified homopolymer PP for injection moulding with decreased flammability. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil forms, guides, co.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 91 T 20 Polypropylene Homopolymer, 20% Micronized Talc FeaturesModified homopolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
|
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latamid 6 H2 G/20-V0 PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Inno-Comp INNOPOL® CS 1-1120 AN 20% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-1120 AN is a 20% talc-filled polypropylene homopolymer compound /PP-H TD20 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 1-1120 AN is develo.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
|
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latan 13 K/30 POM, 30% Carbon Fiber Reinforced Polyoxymethylene (POM) based compound. Carbon fiber. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latan 13 K/30 POM, 30% Carbon Fiber Reinforced Polyoxymethylene (POM) based compound. Carbon fiber. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latene® 7H2-V2HF PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. UL94 V-2 classified, halogens-based flame retardants free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latene® EP 7 TES/30 PP Copolymer, 30% Talc filled Polypropylene copolymer (PPc) based compound. Aesthetic talc. Very good surface appearance. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latigray 53/22-01 CX/25 PP Homopolymer, Impact Modified Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXALEN PPH319FX21 Polypropylene Homopolymer SAXALEN PPH319FX21 is a unfilled Polypropylene - Homopolymer intended for injection molding. It has flame retardant properties and suitable to produce thin-walled parts.Information provided by SAX P.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis HF700SA Polypropylene HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis PS65T20 Polypropylene Compound, Mineral Filled PS65T20 is a 20% mineral filled polypropylene compound intended for injection and back injection molding. This material has excellent balanced mechanical properties and high melt flow rate. Applic.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis ME212U Polypropylene Compound, Mineral Filled ME212U is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: air ducts, air.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 72 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 81 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C... |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -40.0 °C |
7.14 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LASTIROL TR G/10-V1 ES 10% Glass Fiber Polystyrene (PS) Structural Foam Resin (UL94 V-1)
(discontinued * Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latene® 9H TES/30 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Aesthetic talc.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
|
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid.. |