Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 51 T 40 PP, 40% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 81 T 20 PP, 20% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 20% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 82 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% micronized, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitur.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 76 T 20 FRD 5 PP, 20% mineral filling, flame retardant FeaturesModified homopolymer PP for injection moulding, with the content of 20% microground chemically modified talc, retarded with halogen flame retardant Application - electrical industry - termin.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 T 10 PA6, mineral filling FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased modulus in tension - strength of the material. PA matrix reduction. Application eg. for tools, fi.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 Y 35 FRY 7 PA66, 35% mineral filling FeaturesPA 66 for injection moulding, chemically reinforced with 35 % mineral filler and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 /3.2 mm/ in accordance wi.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -40.0 °C |
7.14 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eU |
Polyplastic Armlen® PP MF 15-3 FR Polypropylene Homopolymer, Mineral Filled Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -40.0 °C |
7.14 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eU |
Polyplastic Armlen® PP-2FR Polypropylene, Flame Retardant Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Charpy Impact Unnotched | 1.50 - 1.80 J/cm² @Temperature 23.0 °C |
7.14 - 8.57 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group 2568 AMC Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 51 T 30 Polypropylene Copolymer, 30% Micronized Talc FeaturesModified copolymer PP for injection moulding with the content of 30% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden f.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 91 T 20 Polypropylene Homopolymer, 20% Micronized Talc FeaturesModified homopolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -40.0 °C |
7.14 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LATAN 13 S/30 30% Glass Sphere Reinforced Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Inno-Comp INNOPOL® CS 1-5120 BLH 20% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-5120 BLH is a 20% talc-filled polypropylene homopolymer compound /PP-H TD20 (ISO 1043)/.INNOPOL® CS 1-5120 BLH is recommended especially for producing products, where high stiffn.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
|
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Inno-Comp INNOPOL® CS 1-1120 AN 20% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-1120 AN is a 20% talc-filled polypropylene homopolymer compound /PP-H TD20 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 1-1120 AN is develo.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latan 13 K/30 POM, 30% Carbon Fiber Reinforced Polyoxymethylene (POM) based compound. Carbon fiber. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXALEN PPH319FX21 Polypropylene Homopolymer SAXALEN PPH319FX21 is a unfilled Polypropylene - Homopolymer intended for injection molding. It has flame retardant properties and suitable to produce thin-walled parts.Information provided by SAX P.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis HF700SA Polypropylene HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis PS65T20 Polypropylene Compound, Mineral Filled PS65T20 is a 20% mineral filled polypropylene compound intended for injection and back injection molding. This material has excellent balanced mechanical properties and high melt flow rate. Applic.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis MS64T20 Polypropylene Compound, Mineral Filled MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 91 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 72 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -40.0 °C |
7.14 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LASTIROL TR G/10-V1 ES 10% Glass Fiber Polystyrene (PS) Structural Foam Resin (UL94 V-1)
(discontinued * Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latene® 9H TES/30 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Aesthetic talc.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
|
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -20.0 °C |
7.14 ft-lb/in² @Temperature -4.00 °F |
|
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid.. |