PolyOne Therma-Tech™ LC-5000C TC LCP  (discontinued **)

Category Polymer , Thermoplastic , Liquid Crystal Polymer (LCP) , Liquid Crystal Polymer (LCP), Unfilled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Therma-Tech™ LC-5000C TC LCP  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of thermoplastics. These materials provide the benefits of proprietary conductive additive technologies and the performance of select engineering thermoplastic resins. Therma-Tech compounds have been shown to improve thermal conductivity up to 100-times that of conventional plastics and can be used in a wide range of thermal management applications.
Physical Properties Metric English Comments
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
Water Absorption 0.010 %

@Thickness 3.18 mm,
Time 86400 sec
0.010 %

@Thickness 0.125 in,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.2 MPa
8010 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 0.60 %
0.60 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 17.9 GPa
2600 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 10.3 GPa
1490 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.599 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Thermal Conductivity 2.50 W/m-K
17.4 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 266 °C

@Thickness 6.35 mm
511 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 260 °C

@Thickness 6.35 mm
500 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 - 1.00e+16 ohm-cm
1.00e+15 - 1.00e+16 ohm-cm
ASTM D257
Surface Resistance 1.00e+13 - 1.00e+14 ohm
1.00e+13 - 1.00e+14 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 316 - 341 °C
601 - 646 °F
Mold Temperature 93.3 - 121 °C
200 - 250 °F
Descriptive Properties Value Comments
Features Electrically Insulating
Thermally Conductive
Forms Pellets
Generic Name Liquid Crystal Polymer (LCP)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Automotive Under the Hood
Consumer Applications
Electrical/Electronic Applications
Housings
Industrial Applications