Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 266 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 266 °C

@Thickness 6.35 mm
511 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Therma-Tech™ LC-5000C TC LCP  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Deflection Temperature at 0.46 MPa (66 psi) 266 - 280 °C
510 - 536 °F
Average value: 270 °C Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%..
Deflection Temperature at 0.46 MPa (66 psi) 266 °C
510 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PPA GF30 SL2 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided b..
Deflection Temperature at 0.46 MPa (66 psi) 266 °C
510 °F
Unannealed; ASTM D648
Techmer ES Statiblend® PPS GF23 IM BK 23% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 23% Filler by WeightAdditive: Impact ModifierFeatures: Conductive and Impact ModifiedAppearance: BlackInformation provided..
Deflection Temperature at 0.46 MPa (66 psi) 266 - 301 °C
510 - 573 °F
Average value: 284 °C Grade Count:5
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi..