Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging VEO-111 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Plaskolite Optix® CA-990 Impact Modified Acrylic Resin Injection Molding and Extrusion Grade. Excellent surface gloss. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M5015 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding MR200 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 75.8 MPa | 11000 psi | |
Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite Formerly known as grade MM 1100. Synthetic mica filler. Does not burn. Excellent radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating m.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Polymer Resources ABS-G10 ABS, 10% Glass Reinforced Acrylonitrile Butadiene Styrene, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
PolyOne Edgetek® XT XT-100-BU03 Black Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
PolyOne Lubri-Tech™ AT-000/5T Black Acetal-Copolymer, PTFE Lubricated
(discontinued **) Preliminary DataDescription/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
LNP Lubricomp® GFL-4034 EM M Polysulfone, Milled Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **)& Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Fiberfil® J-60/15/E Polypropylene Homopolymer, 15% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 75.8 MPa | 11000 psi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® PCT2000 PC/PCT Alloy PC/PCT alloy with good balance of physical propertiesAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® PCT2018 PC/PBT Alloy PC/PBT alloy with excellent low temperature impact strengthAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Techmer ES HiFill® HDPE GF25 CC 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Techmer ES Statiblend® PA12 CB Availability: North AmericaForms: PelletsAdditive: Carbon BlackFeatures: ConductiveAppearance: BlackTPCI# 9872105Information provided by TP Composites, Inc. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6 FR HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D-790 |
Axiall HH-2000 Rigid PVC, Molding Georgia Gulf HH-2000 is a high heat/high flow injection molding grade PVC alloy with a price/performance niche between high flow vinyl and utility engineering thermoplastics. It combines excellent .. |
|||
Flexural Strength | 75.8 - 89.6 MPa | 11000 - 13000 psi | |
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D-790 |
Axiall 7055 Rigid PVC, Extrusion Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: WeatherabilityChemicalDurabilityEase of ProcessingToughnessInformat.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D-790 |
Axiall 7181 Rigid PVC, Extrusion Georgia Gulf 7181 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: WeatherabilityImpact StrengthDimensional StabilityFlame Ret.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D-790 |
Axiall 7555 Rigid PVC, Extrusion, Natural Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D-790 |
Axiall 7555 Rigid PVC, Extrusion, White Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D-790 |
Axiall UV-7160 Rigid PVC, Molding Georgia Gulf UV-7160 is a rigid vinyl injection molding compound characterized by excellent flow, toughness, heat stability, color hold and surface appearance. This combination of outstanding attri.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
PolyOne Edgetek® AT-10GF/000 FDA Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation. |