Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D-790 |
Plaskolite Optix® CA - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
PolyOne LubriOne™ AT-000/10T Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D-790 |
Plaskolite Optix® CP - 927 G High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Polymer Resources NY6-IM1 Nylon 6, Impact Modified Nylon 6, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (.. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
Kolon KOCETAL® VT301 Anti-Static Grade Acetal Resin Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
KYDEX® 110 Metallic Thermoplastic Fire-rated Sheet Features:For deep or hard to form parts where good finished detail is requiredMore rigid than most thermoplastics, parts deform less when loadedMeets highest standard for chemical resistance for the.. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KP004AXC Acetal Homopolymer LNP LUBRICOMP* KP004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Techmer ES HiFill FR® ABS GF15 FR-2 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Techmer ES Plaslube® PC-50/TF/22 BK223 Polycarbonate |
|||
Flexural Strength | 75.5 MPa | 11000 psi | ASTM D790 |
Samsung Cheil Industries Starex® SF-0505H MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | |
Cosmic Plastics ID-50 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
Videolar 500 Crystal Polystyrene (GPPS) Designed for injection moldingVery easy flowing grade for fast cycle injection moldingExcellent processability for filling thin partsFeatures: Good strengthGood temperature resistanceExcellent clari.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Westlake Plastics Propylux® CN-F Polypropylene (conductive) Non-sloughing, carbon-fiber-filled material with good chemical resistance, and high strength and stiffness and good temperature resistance to 215F. This material is light weight, easily machined an.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM) TECAFORM™ AH ID is the fist commercially available acetal that is fully detectable by standard metal detection equipment. Exhibiting excellent machinability and a good combination of physical prop.. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ISO 178 |
Denka MALECCA K-095 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Ensinger Tecaform™ Acetal Copolymer - Extruded Products (POM) Tecaform™ is a semi-crystalline thermoplastic offering high strength, stiffness and toughness. It is resistant to hot water, hydrocarbons and solvents, and it posses good bearing and wear properti.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Adell BI-30 Nylon 6, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 75.8 - 145 MPa | 11000 - 21000 psi | |
Bulk Molding Compounds BMC 606 Mineral Filled, Glass Reinforced Polyester Compound BMC 606 is a mineral filled, glass reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good moldability, excellent impact strength,.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D-790 |
Axiall 9113 Rigid PVC, Molding Georgia Gulf 9113 is used for a variety of packages including charcoal lighter fluid, toiletries and household chemicals. It has excellent impact strength.Information provided by Georgia GulfGeorgi.. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ISO 178 |
BASF Ultradur® B 6550 LN PBT Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF |
|||
Flexural Strength | 76.0 MPa | 11000 psi | 2 mm/min; ISO 178 |
Sax Polymers SAXALEN PPC343G20 Polypropylene Copolymer, 20% Glass Filled SAXALEN PPC343G20 is a 20% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |
|||
Flexural Strength | 75.8 MPa | 11000 psi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® PCT2014 PC/PBT Alloy PC/PBT alloy with improved impact strengthAll information provided by LTL Color Compounders, Inc. |