Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne OnForce™ LFT PP-50LGF/001 UV Black Polypropylene Homopolymer (PP Homopolymer)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer PolyOne Corporation
Trade Name OnForce™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne OnForce™ LFT PP-50LGF/001 UV Black Polypropylene Homopolymer (PP Homopolymer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. These products exhibit enhanced physical and mechanical properties versus standard short fiber products. Benefits of LFT compounds include improved impact strength, elastic modulus, and material strength across wide temperature ranges from subambient to highly elevated. Furthermore, LFT compounds have been shown to offer improved performance in the areas of creep and fatigue performance, improved dimensional stability, and exhibit an exceptional surface finish when compared to traditional highly filled short fiber products.LFT compounds can be processed using equipments similar to those used for short fiber products. The mechanical properties depend greatly on the length of the fibers in the moulded part; therefore processing conditions must be set carefully in order to minimize fiber breakage. A low shear process is advised, with low back pressure, low screw speed and low to medium injection speed.Information provided by PolyOne
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Measured on a tensile specimen.; ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
ISO 527-2
Elongation at Break 2.0 %
2.0 %
ISO 527-2
Tensile Modulus 13.5 GPa
1960 ksi
ISO 527-2
Flexural Strength 190 MPa
27600 psi
ISO 178
Flexural Modulus 9.00 GPa
1310 ksi
ISO 178
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179
Gardner Impact 9.60 J
7.08 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
Unannealed; ISO 75-2/A
Deflection Temperature at 8.0 MPa 139 °C
282 °F
Unannealed; ISO 75-2/C
Processing Properties Metric English Comments
Melt Temperature 210 - 230 °C
410 - 446 °F
Mold Temperature 60.0 °C
140 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2.00 hour
2.00 hour
Back Pressure 1.00 MPa
145 psi
Descriptive Properties Value Comments
Features Good UV Resistance
Heat Stabilized
Filler / Reinforcement Long Glass Fiber, 50% Filler by Weight
Forms Pellets
Generic Material PP Homopolymer
Generic Name Polypropylene Homopolymer (PP Homopolymer)
Injection Rate Slow-Moderate
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved