Polymer Property : Gardner Impact = 9.60 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 9.60 J
7.08 ft-lb
ASTM D5420
PolyOne OnForce™ LFT PP-50LGF/001 UV Black Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Gardner Impact 9.60 J
7.08 ft-lb
ASTM D3029
Buckeye Polymers BP RPP 3012 C Polypropylene, 30% Mineral Filled
Applications:Outdoor FurnitureCalcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized thr..