Material Notes:
OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of both raw materials, for example the good processability and soft haptic of a TPE-S with the excellent mechanical properties and abrasion resistance of a TPE-U. OnFlex™-U 5300 compounds are formulated to deliver very good scratch resistance, a wide hardness range and good chemical resistance.Properties are measured using injection molded plaques.Information provided by PolyOne
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ISO 868
Tensile Strength at Break 25.0 MPa
3630 psi
ISO 37
Tensile Stress 4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
ISO 37
9.30 MPa

@Strain 300 %
1350 psi

@Strain 300 %
ISO 37
Elongation at Break 520 %
520 %
ISO 37
Abrasion 57
57
[mm³]; ISO 47469
Processing Properties Metric English Comments
Melt Temperature 170 - 210 °C
338 - 410 °F
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F
Drying Temperature 100 °C
212 °F
Dry Time 2.00 hour
2.00 hour
Descriptive Properties Value Comments
Features Good Abrasion Resistance
Oil Resistant
Scratch Resistant
Forms Pellets
Generic Material TPE
Generic Material Type Thermoplastic Polyurethane Elastomer (TPU)
Generic Name Thermoplastic Elastomer (TPE)
Injection Rate Slow
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Automotive Applications
Consumer Applications
General Purpose
Industrial Applications
Power/Other Tools