Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® PE-40GF/000 NATURAL High Density Polyethylene (HDPE), Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® PE-40GF/000 NATURAL High Density Polyethylene (HDPE), Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Fiber ReinforcedNaturalPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 58.6 MPa
8500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 5.17 GPa
750 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Izod Impact, Notched 1.33 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.50 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
Annealed, 0.125 in bars; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 193 - 221 °C
380 - 430 °F
Molding
Mold Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Descriptive Properties Value Comments