Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® NL-23CF/000 Nylon 6/12, Carbon Fiber Reinforced  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® NL-23CF/000 Nylon 6/12, Carbon Fiber Reinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Water Absorption 0.23 %

@Thickness 3.17 mm
0.23 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 165 MPa
24000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 10.3 GPa
1500 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 296 MPa
43000 psi
ASTM D790
Flexural Modulus 10.3 GPa
1500 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
3.00 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 100 - 10000 ohm-cm
100 - 10000 ohm-cm
ASTM D257
Surface Resistivity per Square 100 - 10000 ohm
100 - 10000 ohm
ASTM D257