Electrical Properties Metric English Comments
Surface Resistivity per Square 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
PolyOne Lubri-Tech™ AT-15CF/5T Acetal-Copolymer, Carbon Fiber Reinforced, PTFE Lubricated  (discontinued **)&l
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Surface Resistivity per Square 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
PolyOne Lubri-Tech™ AS-15CF/15T Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced, PTFE Lubricated &nb
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Surface Resistivity per Square 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
PolyOne Edgetek® AS-20CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Surface Resistivity per Square 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
PolyOne Edgetek® NL-23CF/000 Nylon 6/12, Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation.
Surface Resistivity per Square 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
PolyOne Lubri-Tech™ NL-30CF/10T-2S Nylon 6/12, Carbon Fiber Reinforced, PTFE Lubricated  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Surface Resistivity per Square 100 - 10000 ohm
100 - 10000 ohm
ASTM D648
Techmer ES Electrafil® J-4/25/CF/15 BK PA6/12
Surface Resistivity per Square 100 - 10000 ohm
100 - 10000 ohm
ASTM D648
Techmer ES Electrafil® J-4/25/CF/15 NAT PA6/12
Surface Resistivity per Square 1000 - 10000 ohm
1000 - 10000 ohm
ASTM D648
Techmer ES Electrafil® M-1322 PA66 / PA6
Surface Resistivity per Square 100 - 10000 ohm
100 - 10000 ohm
ASTM D648
Techmer Lehvoss Compounds Luvotech™ J-4/30 BK PA6/12  (discontinued **)
Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated.
Surface Resistivity per Square 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
PolyOne Lubri-Tech™ NI-30CF/10T-2S Nylon 6/10, Carbon Fiber Reinforced, PTFE/Silicone Lubricated  (discontinue
Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Surface Resistivity per Square 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
PolyOne Lubri-Tech™ MP-20CF/15T Modified Polyphenylene Oxide (mPPO), Carbon Fiber Reinforced, PTFE Lubricated  
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Surface Resistivity per Square 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
PolyOne Edgetek® PI-20CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Surface Resistivity per Square 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
PolyOne Edgetek® AM-20CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Surface Resistivity per Square 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
PolyOne Edgetek® AM-20CF-20GF/000 Polyphthalamide (PPA), Glass/Carbon Fiber Filled  (discontinued **)
Description/Features:Glass/Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.