Material Notes:
General purpose neopreneInformation provided by Seals Eastern, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D297, 15
Mechanical Properties Metric English Comments
Hardness, Shore A >= 58
>= 58
ASTM D2240, Type A
65
65
AVG; ASTM D2240, Type A
Tensile Strength at Break >= 13.50 MPa
>= 1958 psi
ASTM D412 Method A
16.15 MPa
2343 psi
AVG; ASTM D412 Method A
Tensile Strength, Yield >= 1.06 MPa
>= 154 psi
Stress at Elongation M50; ASTM D412 Method A
1.39 MPa
202 psi
AVG Stress at Elongation M50; ASTM D412 Method A
>= 1.87 MPa
>= 271 psi
Stress at Elongation M100; ASTM D412 Method A
2.62 MPa
380 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Elongation at Break 264 %
264 %
AVG; ASTM D412 Method A
>= 291 %
>= 291 %
ASTM D412 Method A
Modulus of Elasticity 0.00574 GPa
0.832 ksi
ASTM D412 Method A
Shear Modulus 0.00191 GPa
0.277 ksi
ASTM D412 Method A
Secant Modulus 0.00539 GPa
0.782 ksi
ASTM D412 Method A
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -40.0 °C
-40.0 °F
ASTM D1329
Descriptive Properties Value Comments
Strain Energy / Unit Volume at 20% Elongation (psi) 15