Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 296 MPa | 43000 psi | ASTM D790 |
PolyOne Edgetek® ES-40CF/000 Polyethersulfone - 40% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Flexural Strength | 296 MPa | 43000 psi | ASTM D790 |
PolyOne Edgetek® NL-23CF/000 Nylon 6/12, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 296 MPa | 43000 psi | ASTM D790 |
Techmer ES Electrafil® J-4/25/CF/15 BK PA6/12 |
|||
Flexural Strength | 296 MPa | 43000 psi | ASTM D790 |
Techmer ES Electrafil® J-4/25/CF/15 NAT PA6/12 |
|||
Flexural Strength | 296 MPa | 43000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF43 L BK001 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackTPCI# 7176101Information provi.. |
|||
Flexural Strength | 296 MPa | 43000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF43 L BKN001 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackProcessing Method: Injection M.. |
|||
Flexural Strength | 296 MPa | 43000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF43 LE BK 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant Features: Lubricated and Low ExtractablesAppearance: BlackInformatio.. |
|||
Flexural Strength | 296 MPa | 43000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF45 L BK 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackProcessing Method: Injection M.. |
|||
Flexural Strength | 296 MPa | 43000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF45 TL10 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: PTFE Lubricant (10%)Features: LubricatedInformation provided by TP Composites.. |
|||
Flexural Strength | 296 MPa | 43000 psi | ASTM D790 |
Techmer ES Electrablend® PA6 CF30 TL10 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Conductive and LubricatedAppearance: BlackInform.. |
|||
Flexural Strength | 296 MPa | 43000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF50 FR BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 296 MPa | 43000 psi | ASTM D790 |
Asahi Kasei Thermylon® LSG-440A 60% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |