Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® ET6620-0020 FRV0 Polyamide 66 (Nylon 66)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® ET6620-0020 FRV0 Polyamide 66 (Nylon 66).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Water Absorption 0.30 %

@Temperature 23.0 °C
0.30 %

@Temperature 73.4 °F
@ 24 hrs; Internal Method
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 117 MPa
17000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 8.27 GPa
1200 ksi
ASTM D638
Flexural Strength 159 MPa
23100 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.350 J/cm
0.656 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 187 °C

@Thickness 3.18 mm
369 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0626 in
UL 94
V-0

@Thickness 3.18 mm
V-0

@Thickness 0.125 in
UL 94
Descriptive Properties Value Comments
Appearance Black
Features Flame Retardant
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
South America
UL File Number E41877