Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
PolyOne Nymax™ GF 600 A 33 HS7 DX9 Black Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Rogers Corporation Syron™ 7000 Thermoplastic Circuit Material SYRON™ 7000 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7000 is thermally stable, with a .. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
PolyOne Nymax™ GF 600 A 33 Black 13 Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
PolyOne Nymax™ GF 600 A 33 Black 28 V Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Quadrant EPP Duratron® T7130 PAI Polyamide-imide, carbon fiber reinforced, extruded (ASTM Product Data Sheet) |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ SF-25GF/13T-2S Polyphenylene Sulfide (PPS), Glass Filled, PTFE/Silicone Lubricated
(disco Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ NL-30GF/15T Nylon 6/12, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)Information provided by PolyOne Corporation. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Fibre Glast 90L Isophthalic Polyester Resin (Laminate Properties) Description:#90 Isophthalic Polyester Resin is perfect for making dimensionally stable polyester molds, corrosive service part fabrication, and as a durable repair material for tank linings. #90 per.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 (Asia Pacific) LNP* Lubricomp* RFL34 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66 LNP* STAT-KON* RE002 is a compound based on Nylon 66 resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 8.27 GPa @Temperature -60.0 °C |
1200 ksi @Temperature -76.0 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Ensinger Tecapeek® XP-106 Compression Molded PEEK Compound, 40% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Ensinger Tecapeek® XP-91 Compression Molded PEEK Compound, 30% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Ensinger Tecapeek® XP-99 Compression Molded PEEK Compound, Bearing Grade Material with 7% Graphite, 8% PTFE, and 15% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Ensinger Tecatron® XP-82 Compression Molded PPS Compound, Filled with 15% PTFE and 30% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PI-20GF/000 Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Solvay Specialty Polymers Parmax® 1200 Self-Reinforcing Polyethersulfone
(discontinued **) PARMAX 1200 self-reinforcing polymer (SRP) is an ultra-high performance amorphous, melt-processable engineering thermoplastic. The unique properties of this material are due primarily to the inheren.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Plenco 6554 Phenolic, Granular, Compression Molded
(discontinued **) Two-Stage Phenolic. PLENCO 06554 is an organic reinforced phenolic molding compound modified with PTFE to offer improved coefficient of friction values. 06554 is available in black.Information supp.. |