Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 159 MPa | 23100 psi | ASTM D790 |
PolyOne LubriOne™ SF-30GF/15T Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 159 MPa | 23100 psi | |
Pyrotek TS-106 Thermoset Electrical Insulation Product Glass reinforcement, Polyester resin, Tan / Red color. High heat resistance. UL recognized.Information provided by Pyrotek. |
|||
Flexural Strength | 159 MPa | 23100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Flexural Strength | 159 MPa | 23100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Flexural Strength | 159 MPa | 23100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Flexural Strength | 159 MPa | 23100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Flexural Strength | 159 MPa | 23100 psi | |
Pyrotek TS-82 Thermoset Electrical Insulation Product (Nema Grade: XXX) Paper reinforcement, Phenolic Resin, Natural Color. High humidity resistance, Excellent resistance to splitting.Information provided by Pyrotek. |
|||
Flexural Strength | 159 MPa | 23100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Flexural Strength | 159 MPa | 23100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Flexural Strength | 159 MPa | 23100 psi | ASTM D790 |
PolyOne Edgetek® ET6620-0020 FRV0 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Strength | 159 MPa | 23100 psi | ASTM D790 |
PolyOne Geon™ 81530 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 159 MPa | 23100 psi | ASTM D790 |
PolyOne Stat-Tech™ OC-0307081 Black Acrylonitrile Butadiene Styrene + PC (ABS+PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Flexural Strength | 159 MPa | 23100 psi | ASTM D790 |
Lucent Polymers LPB-130 Polybutylene Terephthalate, 30% Glass Fiber/Mineral Reinforced, Low Warp Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 159 MPa | 23100 psi | |
Haysite ETS Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) A NEMA GPO-1 economy grade fiberglass mat reinforced thermoset polyester molded sheet. ETS is an IEEE Class B 130ºC electrical/160ºC mechanical material with good punching characteristics. Typ.. |
|||
Flexural Strength | 159 MPa | 23100 psi | |
Haysite HCR-100 Corrosion Resistant Polyester/Glass Sheet A general purpose isophthalic polyester sheet with flame retardants and ultraviolet inhibitors. Standard color is gray. |
|||
Flexural Strength | 159 MPa | 23100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC (Asia Pacific) LNP* Stat-Kon* DE002 is a Polycarbonate containing Carbon Fiber. |
|||
Flexural Strength | 159 MPa | 23100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Flexural Strength | 159 MPa | 23100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Flexural Strength | 159 MPa | 23100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon DEF13 PC LNP* Stat-kon* DEF13 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Flexural Strength | 159 MPa | 23100 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Clean Compounding System, Electrically Conductive, Wear Resistant, Ea.. |
|||
Flexural Strength | 159 MPa | 23100 psi | ASTM D790 |
Solvay Specialty Polymers Ryton® XE5515BL Polyphenylene Sulfide Alloy (PPS Alloy), 15% Glass Fiber Ryton® XE5515BL 15% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength and chemical resistance at elevated temperatures and is suitable for extrusi.. |
|||
Flexural Strength | 159 MPa | 23100 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC (Asia Pacific) LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features of this material include: Clean Compounding System. |
|||
Flexural Strength | 159 MPa | 23100 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing 20% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |
|||
Flexural Strength | 159 MPa | 23100 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 159 MPa | 23100 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MF006SXP PP LNP THERMOCOMP* MF006SXP is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Flexural Strength | 159 MPa | 23100 psi | 1.97" span; ASTM D790 |
Westlake Plastics Tempalux® 5000 Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high heat resistance, high strength at elevated temperatures, hi.. |
|||
Flexural Strength | 159 MPa | 23100 psi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |
|||
Flexural Strength | 159 MPa | 23100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON PX05047 PA 6 (Europe-Africa-Middle East) LNP* Stat-kon* PX05047 is a compound based on PA 6 resin containing Carbon Fiber, Proprietary Filler (s). Added features include: Electrically Conductive, High Impact. |
|||
Flexural Strength | 159 MPa | 23100 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Asia Pacific) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |