Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 17000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 117 MPa
17000 psi
ASTM D-638
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Tensile Strength 117 MPa
17000 psi
ASTM D-638
PlastiComp Complet® LGF40 - PP Homopolymer Polypropylene, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% long glass fiber reinforcementInformation provided by PlastiCom..
Tensile Strength 117 MPa
17000 psi
ASTM D-638
PlastiComp Complet® LGF60 - PP Homopolymer Polypropylene, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 60% long glass fiber reinforcementInformation provided by PlastiCom..
Tensile Strength 117 MPa
17000 psi
ASTM D638
Quadrant EPP Duratron® PEI U1000 LSG Polyetherimide, unfilled, extruded, Biocompatibility tested (ASTM Product Data Sheet)
Duratron® U1000 (Formerly Ultem® 1000) polyetherimide is an amorphous, high-performance polymer with exceptional flame and heat resistance. It performs continuously to 340°F (171°C), making it..
Tensile Strength 117 MPa
17000 psi
ASTM D638
PolyOne Edgetek® ET6620-0020 FRV0 Polyamide 66 (Nylon 66)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Tensile Strength 117 MPa
17000 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughness-re..
Tensile Strength 117 MPa
17000 psi
ASTM D638
Quadrant EPP Duratron® PEI U1000 Extruded Unfilled Polyetherimide (ASTM Product Data Sheet)
Tensile Strength 117 MPa
17000 psi
ASTM D638
Quadrant EPP Duratron® PEI U2300 Extruded 30% Glass Reinforced Polyetherimide (ASTM Product Data Sheet)
Tensile Strength 117 MPa
17000 psi
ASTM D638
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with ..
Tensile Strength 117.2 MPa
17000 psi
ASTM D 638
MRC Polymers MAXNITEâ„¢ 550 GF30 PET, 30% Glass Mineral Reinforced
Information provided by MRC Polymers Inc.
Tensile Strength 117 MPa
17000 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK), 13% Glass Fiber
KetaSpire® KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughnes..
Tensile Strength 117 MPa
17000 psi
ASTM D638
Techmer ES HiFill FR® PA6 GF25 FR IM 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Flame Retardant and Impact ModifierFeatures: Flame Retardant and Impact Modifi..
Tensile Strength 117 MPa
17000 psi
ASTM D638
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin..
Tensile Strength 117 MPa
17000 psi
ASTM D638
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w..
Tensile Strength 117 MPa
17000 psi
ASTM D638
Techmer ES Luriblend® PA6/10 GF30 TS15 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE+ Silicone LubricantFeatures: Lubricated, Heat Stabilizer and Good W..
Tensile Strength 117 MPa
17000 psi
DIN EN ISO 527
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut..
Tensile Strength 117 MPa
17000 psi
ASTM D638
Ensinger Tecapeek® XP-119 Compression Molded PEEK Compound, 10% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Tensile Strength 117 MPa

@Temperature 150 °C
17000 psi

@Temperature 302 °F
ASTM D638
DuPont Performance Polymers VESPEL TP-8541 Polyimide
Thermoplastic parts from filled PI (polyimide) for high mechanical properties and impact performance in high temperature environmentsInformation provided by DuPont Performance Polymers
Tensile Strength 117 MPa
17000 psi
ASTM D638
Aaron Industries AAROPRENE® G/MFN 6002 Glass and Mineral Filled Nylon 6
AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified.
Tensile Strength 117 MPa
17000 psi
ASTM D-638
PlastiComp Complet® LGF20 - PA66 Nylon 66, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc.
Tensile Strength 117 MPa

@Temperature 22.8 °C
17000 psi

@Temperature 73.0 °F
ASTM D638
Quadrant EPP Duratron® U2200 PEI Extruded 20% Glass Reinforced Polyetherimide
Copyright © lookpolymers.com All Rights Reserved