PolyOne Edgetek® AT-000/07SS Copolymer Acetal - 7% Stainless Steel Fiber  (discontinued **)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® AT-000/07SS Copolymer Acetal - 7% Stainless Steel Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.498 g/cc
0.05412 lb/in³
ASTM D792
Water Absorption 0.10 %
0.10 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.010 - 0.020 cm/cm

@Thickness 3.17 mm
0.010 - 0.020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 59.0 MPa
8560 psi
ASTM D638
Elongation at Break 1.0 - 3.0 %
1.0 - 3.0 %
ASTM D638
Tensile Modulus 2.60 GPa
377 ksi
ASTM D638
Flexural Yield Strength 97.0 MPa
14100 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 0.430 - 0.590 J/cm

@Thickness 6.35 mm
0.806 - 1.11 ft-lb/in

@Thickness 0.250 in
ASTM D256
Electrical Properties Metric English Comments
Electrical Resistivity 1.00 - 1000 ohm-cm
1.00 - 1000 ohm-cm
ASTM D257
Surface Resistance 1.0 - 1000 ohm
1.0 - 1000 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 188 - 227 °C
370 - 441 °F
Stock
Mold Temperature 54.0 - 71.0 °C
129 - 160 °F
Drying Temperature 71.0 °C
160 °F