Polimeri Europa Eraclene® MR 80 High Density Polyethylene - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Eraclene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Eraclene® MR 80 High Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eraclene MR 80 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. Eraclene MR 80 shows a good balance between processability and mechanical properties.Main Applications: Eraclene MR 80 is specifically designed for houseware and thin-walled containers.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.954 g/cc
0.954 g/cc
ISO 1183
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 190 °C
18 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ISO 868/A
Tensile Strength at Break 14.0 MPa
2030 psi
ISO 527
Tensile Strength, Yield 27.0 MPa
3920 psi
ISO 527
Elongation at Break 200 %
200 %
ISO 527
Flexural Modulus 1.25 GPa
181 ksi
ISO 178
Izod Impact, Notched 0.450 J/cm
0.843 ft-lb/in
ISO 180/A
Thermal Properties Metric English Comments
Melting Point 135 °C
275 °F
Internal method
Vicat Softening Point 126 °C

@Load 1.00 kg
259 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746