Zeon Chemicals HyTemp® 4051EP AR Polyacrylate Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name HyTemp®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals HyTemp® 4051EP AR Polyacrylate Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HyTemp 4051EP contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat and compression set resistance.Easy processing version of HyTemp 4051.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Viscosity <= 13000 cP
<= 13000 cP
Unmilled Cement; Zeon Test #328
Mooney Viscosity 35 - 47

@Temperature 100 °C
35 - 47

@Temperature 212 °F
(1+4); Zeon Test #404
Ash <= 0.50 %
<= 0.50 %
Zeon Test #873
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -18.0 °C
-0.400 °F
Gehman T100
Descriptive Properties Value Comments
% Volume Swell 11
Curesite Dual
Heat Loss (%) Max 0.7