Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Nylene® 406F Nylon 6, 50% RH Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling molding resin.
.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Nylene® 409 Nylon 6, 50% RH Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid m.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® BB 76 High Density Polyethylene - Blow Molding Eraclene BB 76 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 30 liters.Er.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® MG37EPX ABS ABS plating grade optimized for a broad processing window for both painted and plated applications. NSF standard 61 compliant (80 sq in/L) |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -30.0 °C |
4.68 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Izod Impact, Notched | >= 2.50 J/cm | >= 4.68 ft-lb/in | blow molding |
Reliance Industries Polypropylene Impact Copolymer Typical properties of Reliance - Repol Polypropylene grades. Properties depend on rubber content, presence of nucleating agent, MFIInformation provided by Reliance Industries |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CM8622 PC+ABS (Europe-Africa-Middle East) CYCOLOY* CM8622 is a high heat PC/ABS blend offering high modulus, low CTE and good |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Ineos Nova Styrosun® 6600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -20.0 °C |
4.68 ft-lb/in @Temperature -4.00 °F |
BS 2782.306A |
Micropol Isoplas P651 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Izod Impact, Notched | 2.50 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
4.68 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, Dry as Molded Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Izod Impact, Notched | 2.50 J/cm @Thickness 3.17 mm |
4.68 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Hannam Chemical Hanalac 750 ABS, General Purpose FDA Approved. Good combination of impact strength, rigidity, gloss, heat resistance, processability, and thermal stability. May be injection molded. Its broad range of applications include: elect.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256A |
LyondellBasell Astryn SD068-4 Polypropylene Copolymer, 40% Calcium Carbonate Key Features: fractional melt flow, high modulus, mineral-filled, blow molding and extrusion grade polypropylene copolymer, good melt strength, excellent processability, excellent impact and stiffne.. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -20.0 °C |
4.68 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL STN15HF PPE+PS (Asia Pacific) Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Styrolution Luran® S 778 Q42 Colored ASA Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan.. |
|||
Izod Impact, Notched | 2.50 J/cm @Thickness 3.17 mm |
4.68 ft-lb/in @Thickness 0.125 in |
ASTM Test |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX1278 PPE+PS Primarily EXTRUSION material. Automotive. Passes FMVSS 302. Heat resistance of 130 C (266 F). |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 (Asia Pacific) LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder, Impact Modifier. Added features of this material include: Electrically Conductive, High Impact. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Unitika M1030B PA6, Conditioned Nano composite nylonInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA865G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RA844 Nylon 6.6, UV Stabilized Impact modified, UV and heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P50B11 Homopolymer Polypropylene, Chemically Coupled 50% LGF A chemically coupled 50% LGF reinforced black PP, heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P50N01 Homopolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber A CHEMICALLY COUPLED 50% LONG GLASS FIBER REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamShine PV507 ABS, Flame Retardant Flame retardant ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTough PZ500 Polycarbonate, Flame Retardant Flame retardant polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
UBE UBESTA® 3035JX47 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: conductiveInformation provided by UBE. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -30.0 °C |
4.68 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |