Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 0.40 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Eraclene® BB 76 High Density Polyethylene - Blow Molding
Eraclene BB 76 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 30 liters.Er..
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Premix Thermoplastics PRE-ELEC® PP 1391 Conductive Thermoplastic Compound
PRE-ELEC® PP 1391 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Melt Flow 0.40 - 0.60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 - 0.60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4142L (424F5) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.40 - 0.60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 - 0.60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4143L (424F5) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.40 - 0.60 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.40 - 0.60 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 6751E (516H5) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.40 - 0.60 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.40 - 0.60 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 6752E (516H5) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.40 - 0.70 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.40 - 0.70 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238/L
NIZHNEKAMSKNEFTEKHIM PP 1532B (YD50G) Propylene Homopolymer
Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P..
Melt Flow 0.40 - 0.70 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.40 - 0.70 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238/L
NIZHNEKAMSKNEFTEKHIM PP 4132B (PA14D) Propylene and Ethylene Copolymer
Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates very high long-term thermal stability, thermal-oxidative degradation r..
Melt Flow 0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
SABIC PP 651H Polypropylene Random Copolymer for PIPE
Product Description: PP 651H is specially designed for transport of hot and cold drinking water. This grade is highly heat stabilized and specially formulated for extraction resistance.Typical App..
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Imerys ImerPlastâ„¢ 10WPCT Recycled Polyolefin Resin
A black, UV stabilized, recycled resin with no significant odor, for compounding with wood flour for extruded decking applications. With added reinforcing filler and wood flour dispersant, ImerPlast..
Melt Flow 0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Global MB-6366 High Density Polyethylene
Description-high density for high quality, excellent creep & chemical resistanceApplications-drinking water pipe, industrial pipe, sewer pipeInformation provided by Global Polymers Corporation.
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Kuraray SEPTON® S2104 Thermoplastic Rubber
SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi..
Melt Flow 0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) HB5510 High Density Polyethylene
HB-5510 is a high molecular weight high density polyethylene.Applications: extrusion large blow moldings, jerry cans, film and blown bags.Information provided by Iran Petrochemical Commercial Co.
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Borealis Borstar® FB4250T LLDPE for Blown Film
Borstar FB4250 is well suited for a wide range of film applications due to its properties. The well balanced mechanical properties will improve the functionality of the films or allow for material ..
Melt Flow 0.40 g/10 min

@Load 2.16 kg
0.40 g/10 min

@Load 4.76 lb
ASTM D1238
Borealis Borstar® HE6081 Black Track Resistant HD Polyethylene Based Compound for Jacketing of Fiber Optical Cable
Borstar HE6081 is based on high-density polyethylene and has a specially designed additive package to give excellent track resistance. It is also well protected against UV degradation in order to e..
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Borealis Borstar® BB2581 HDPE for Blow Molding
Borstar BB2581 is a high-density polyethylene intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR).Borstar BB2581 is recommended for h..
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Borealis Borstar® FB4230 LLDPE for Film
Borstar FB4250T is a high molecular weight linear low density polyethylene grade combining good extrusion properties, excellent draw properties and good mechanical strength. Film made from Borstar ..
Melt Flow 0.40 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.40 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Chi Mei Polylac® PA-709S ABS - Extrusion
Super Impact Extrusion
Melt Flow 0.40 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.40 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Entec Hylac® EX18 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Melt Flow 0.40 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.40 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS TM 40
Description: Heat Resistant Grade, Ultra High HeatInformation provided by Diamond Polymers, Inc.
Melt Flow 0.40 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.40 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ASA T-110
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc.
Melt Flow 0.40 g/10 min

@Load 3.80 kg,
Temperature 230 °C
0.40 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Diamond Polymers Centrex® HGM Automotive Grade, Injection Molding Grade
Centrex HGM resin is an exceptionally high-gloss grade of ASA (acrylonitrile-styrene-acrylate). This injection molding grade has excellent gloss retention, excellent resistance to chemicals and high..
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 220 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 428 °F
ISO 1133
DuPont Performance Polymers Hytrel® HTR237BG BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal dur..
Melt Flow 0.40 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.40 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS/PC 9801
Description: Injection Molding Grade, High Impact, High HeatInformation provided by Diamond Polymers, Inc.
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Borealis Borstar® FB4370 Medium Density Polyethylene
Borstar® FB4370 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Applications: Borstar® FB4370 has been developed especially for ap..