Plenco 7200 Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7200 Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 07200 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength, good powder properties and excellent cosmetic properties. UL recognized under component file E40654. 07200 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.530 g/cc
0.0191 lb/in³
ASTM D1895
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.43 %
0.43 %
ASTM D570
Linear Mold Shrinkage 0.0087 cm/cm
0.0087 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 85
85
ASTM D785
Tensile Strength, Ultimate 43.0 MPa
6240 psi
ASTM D638
Elongation at Break 0.62 %
0.62 %
ASTM D638
Tensile Modulus 8.10 GPa
1170 ksi
ASTM D638
Flexural Strength 66.0 MPa
9570 psi
ASTM D790
Flexural Modulus 6.70 GPa
972 ksi
ASTM D790
Compressive Strength 205 MPa
29700 psi
ASTM D695
Izod Impact, Notched 0.223 J/cm
0.418 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.226 J/cm²
1.08 ft-lb/in²
ASTM D256
Impact 157
157
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 193 °C
379 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 163 °C
325 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Shrinkage 0.43 %
0.43 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.70e+11 ohm-cm
1.70e+11 ohm-cm
ASTM D247
Dielectric Constant 5.4
5.4
ASTM D150
Dielectric Strength 9.60 kV/mm
244 kV/in
Short Time; ASTM D149
Dissipation Factor 0.059
0.059
ASTM D150
Arc Resistance 76 sec
76 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638