Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0087 cm/cm | 0.0087 in/in | ASTM D955 |
RheTech Products RCT140-01A 40% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC ductworkI/P componentsFuse panel assembliesUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0087 cm/cm | 0.0087 in/in | ASTM D955 |
North Wood Plastics Polypropylene with 20% Wood Fiber, Molding Grade Data provided by North Wood Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0087 cm/cm | 0.0087 in/in | ASTM D955 |
Plenco 7200 Phenolic, Granular, Transfer Molded PLENCO 07200 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength, good powder properties and excellent cosmetic properties. UL recognized under component .. |