Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | 4.0 mm thick, 10.0 mm wide molded rod; ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 7300 PRE-ELEC ESD 7300 is a static dissipative thermoplastic compound based on PC/PBT. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7300 has been developed for inj.. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ASTM D638 |
Proto3000 Duraform® PA Selective Laser Sintering (SLS®) Prototyping Polymer Description: Durable polyamide (nylon) material for real-world physical testing and functional useFeatures: Excellent surface resolution and feature detailEasy-to-processCompliant with USP Class VI .. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ASTM D638 |
Rotuba H2 Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ASTM D638 |
Ineos Nova Zylar® 330 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Clarity and stiffness Good heat distortion resistance Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class .. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ISO 527-2 |
NOVA Chemicals DYLARK® 238 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Tensile Strength, Ultimate | 43.0 MPa @Temperature 90.0 °C |
6240 psi @Temperature 194 °F |
ISO 527 |
LATI LATAN 13 G/15 15% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ASTM D638 |
Global R-1760 High Density Polyethylene, Injection Molding Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- auto parts, bottles, housewares, drums, containers, bottlesMeets FDA requirements as listed in.. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Therma-Tech™ NJC-5000 TC NATURAL Nylon 12
(discontinued **) Information provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | |
Kuraray HYBRAR® PS1 Thermoplastic Rubber-Polystyrene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | |
Haysite 18600 Polyester BMC, 15% Glass Reinforced The 18600 series bulk molding compound can be compression, transfer, or injection molded. Formulated with a high temperature resin system, this grade exhibits exceptional retention of physical and e.. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ASTM D638 |
Plenco 1501 Polyester, Briquette, Compression Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ASTM D638 |
Plenco 7200 Phenolic, Granular, Transfer Molded PLENCO 07200 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength, good powder properties and excellent cosmetic properties. UL recognized under component .. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ASTM D638 |
Plenco 7321 Phenolic, Granular, Transfer Molded PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon.. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | DIN 53504 |
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | DIN 53504 |
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ISO 37 |
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ISO 527-1, 2 |
Polyplastics Duranex® CA7200NX Polybutylene Terephthalate (PBT), Antistatic DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ASTM D638 |
3D Systems DuraForm® PA Nylon for SLS® Systems For use with all selective laser sintering (SLS®) systems.ApplicationsComplex, thin-wall ductworkMotorsportsAerospaceHousings and enclosuresImpellers and connectorsConsumer sporting goodsVehicle da.. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ASTM D412 |
BASF Elastollan® S60D Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv.. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | XY; ASTM D638 |
ALM PA 605-A Filled Nylon 12 Prototyping Polymer 50% Aluminum filled nylon 12 that can produce accurate parts with excellent part strength and surface detail.Drop in replacement for other commercially available 50% aluminum filled materials with a.. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ATSM D638 |
Ashley Polymers Ashlene® 626SB Nylon 6 Copolymer A flexible nylon copolymer, heat stabilized, in black, for tubing and other extrusion applications.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ASTM D638 |
A. Schulman ComAlloy Comshield® 220 ABS, Electrically Conductive - Carbon Black Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ASTM D412 |
BASF Elastollan® C-60D Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fue.. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ASTM D638 |
Global NM-3255 High Density Polyethylene, Yarn/Tape Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- ropes, fishing nets, wire & cable insulators, auto parts, pipesInformation provided by Global .. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ASTM D638 |
Eastman Tenite Acetate 109E3V36324 Clear, Trsp Cellulose Acetate
(discontinued **) Plasticizer 24%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.2% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Ultimate | 43.0 MPa | 6240 psi | ASTM D638 |
Plenco 7552 Phenolic, Nodular, Injection Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |