Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | <= 66.0 MPa | <= 9570 psi | ISO 178 |
Polykemi AB POLYabs N00 LG ABS, Low Gloss Information provided by Polykemi AB |
|||
Flexural Strength | <= 66.0 MPa | <= 9570 psi | ISO 178 |
Polykemi AB POLYabs XX0 ABS, Extrusion Grade Information provided by Polykemi AB |
|||
Flexural Strength | <= 66.0 MPa | <= 9570 psi | ISO 178 |
Polykemi AB POLYshine PBT D611 PBT Information provided by Polykemi AB |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Europe-Africa-Middle East) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Eastar 5445 PCTG Copolyester, Injection Molded
(discontinued **) Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | 2mm/min; ASTM D790 |
Kingfa FW-620 Flame Retardant ABS Features:UL 94 V-0 @ 1.5-3.0mmWeather resistanceHeat resistanceGood surfaceApplications:Injection moldingOA deviceChargerTransformerInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | 2mm/min; ASTM D790 |
Kingfa HP-126 Modified ABS Features:UL94 HB @ 1.6-3.0mmHigh impact resistanceHigh flowApplications:LCD cabinetLarge thin-wall partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Flexural Strength | >= 66.0 MPa | >= 9570 psi | |
MarkeTech Repton EXP 48 Cordierite Mg-Al-Si Oxide REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
Ineos ABS Lustran® 288 ABS, Injection Molding Grade Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® 152WG Capped Wood Grain Thermoplastic Sheet Features:Super tough, durableHigh extensibility, rigidity, abrasion resistance and fire retardancyMore rigid than most thermoplastics, parts deform less when loadedOutstanding resistance to breakage.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® 311 MB Co-Extruded High Impact Fire-Rated Thermoplastic Sheet with Microban® Antimicrobial Features:Color-matched cap, black or off-white substrateThickness ranging from 1.5 mm to 8.9 mmToughness and durabilityEasy to form with good part definitionChemical resistantFire retardantExcellent.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® 331/331d Co-Extruded High Impact Fire Rated Thermoplastic Sheet with Weatherable Acrylic Film Cap KYDEX® 331 is a co-extruded high impact fire rated thermoplastic sheet with a weatherable cap that offers superior performance for thermoforming. It can also be used as an impact resistant surfa.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
SABIC Innovative Plastics NORYL STN15 PPE+HIPS (Asia Pacific) PPE+HIPS Unfilled Auto Interior |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM Test |
Styrolution Luran® S 757 G ASA Luran S 757 G is an easy flowing injection molding ASA grade with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
Styrolution Novodur® 530 ABS Novodur 530 is an extrusion grade optimized for sheet applications. It has high impact properties, high modulus and good thermoforming.Information provided by Styrolution |
|||
Flexural Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MX06403 PP LNP* THERMOCOMP* MX06403 is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized, UV Stabilized. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM Test |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Plenco 1500 Polyester, Granular, Compression Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Plenco 7200 Phenolic, Granular, Transfer Molded PLENCO 07200 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength, good powder properties and excellent cosmetic properties. UL recognized under component .. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Toyobo T-661 Nylon 66, Standard Grade (Conditioned) Features: Non-reinforced, Standard GradeInformation provided by Toyobo. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
Unitika M1030DH PA6, Conditioned Nano composite nylonInformation provided by Unitika Ltd. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
Polyplastics Duranex® CA7200NX Polybutylene Terephthalate (PBT), Antistatic DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Eastar DN010 Copolyester Eastar Copolyester DN010 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN010 contains no mold release.Applications.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Eastar DN114 Copolyester, Natural Applications:LightingProduct Description: Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage. DN1.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Eastar GN120 Copolyester Applications:AppliancesConsumer electronicsPersonal care and cosmeticsStationary suppliesKey Attributes:High clarity and transparencyHigh flow copolyesterToughProduct Description: Eastar GN120 Cop.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
Chi Mei Polylac® PA-747F ABS - Extrusion Refrigerator |
|||
Flexural Strength | 66.0 MPa @Thickness 3.17 mm |
9570 psi @Thickness 0.125 in |
5% strain; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABSPC 7801E ABS/PC Extrusion Grade, High Impact, High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |