Teknor Apex Flexalloy® 3501-35-NT Polyvinyl Chloride Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Vinyl (PVC)
Manufacturer Teknor Apex Company
Trade Name Flexalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Flexalloy® 3501-35-NT Polyvinyl Chloride Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppearance-ClearInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
15 seconds; ASTM D2240
Tensile Strength, Yield 1.79 MPa
260 psi
100%; ASTM D412
4.83 MPa
700 psi
3; ASTM D412
6.83 MPa
990 psi
ASTM D412
Elongation at Break 370 %
370 %
ASTM D412
Tear Strength Test 100
100
in psi, Die C; ASTM D624
Compression Set 12 %
12 %
73°F, 22 hr.; ASTM D395
54 %
54 %
158°F, 22 hr.; ASTM D395
68 %
68 %
212°F, 22 hr.; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -59.0 °C
-74.2 °F
ASTM D746