Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | Loose |
Nyco NYAD® 5000 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | Loose |
Nyco NYGLOS® M15 Wollastonite High aspect ratio grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal perf.. |
|||
Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons CORAX® N 772 ASTM Carbon Black Standard grade of furnace black in accordance with the requirements of ASTM D 1765Soft Black - carcass grade, semi-reinforcing carbon blackInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.529 - 0.593 g/cc | 0.0191 - 0.0214 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu.. |
|||
Bulk Density | 0.530 - 0.610 g/cc | 0.0191 - 0.0220 lb/in³ | |
JPJ Technologies DG-700 PVC Information provided by JPJ Technologies |
|||
Bulk Density | 0.530 - 0.610 g/cc | 0.0191 - 0.0220 lb/in³ | |
JPJ Technologies DG-1000 PVC Information provided by JPJ Technologies |
|||
Bulk Density | 0.529 g/cc | 0.0191 lb/in³ | As Supplied |
Skamol Group Skamol M-20 Insulating Mortar SKAMOL insulating mortars have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Dry-mix mortars designed for use with Skamol insulating bricks/blocks and slab grad.. |
|||
Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | DIN 53466 |
Silon Taborex TA 1108 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1108 HD is a crosslinkable compound according to the “SIOPLAS-SYSTEMâ€; made by a Silane grafted ethylene copolymer known as the graft and a Masterbatch containing the crosslinki.. |
|||
Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | ASTM D1895 |
Plenco 7200 Phenolic, Granular, Transfer Molded PLENCO 07200 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength, good powder properties and excellent cosmetic properties. UL recognized under component .. |
|||
Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | ASTM D1895 |
Westlake 1185 PVC Westlake PVC 1185 resin is a low molecular weight resin with excellent clarity designed for applications such as blow molding or where high plasticizer uptake is required.Information provided by Wes.. |
|||
Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | ASTM D1895 |
Westlake 1195 PVC Westlake PVC 1195 resin is a low molecular weight resin designed for rigid injection molding, calendering, sheet extrusion, and blow molding.Information provided by Westlake Chemical Corporation |
|||
Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | |
Daikin NEOFLON NC-1500 FEP Coating Powder, White NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: Up to a thickness of 100 microns per single coat.Proc.. |
|||
Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | |
Daikin NEOFLON NC-1539 FEP Coating Powder, Gray NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: Multiple coats, up to 2,000 microns.Processing Method.. |
|||
Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | ASTM D1895 |
Equate EFDC-7050 LLDPE Film Extrusion Resin EFDC-7050 is a linear low-density polyethylene resin for tubular blown film extrusion. Films extruded from EFDC-7050 have good toughness and high tensile strength and puncture resistance. The produc.. |
|||
Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | ASTM D1895 |
Equate EFDC-7087 LLDPE Film Extrusion Resin EFDC-7087 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from EFDC-7087 have good toughness, high tensile strength and outstanding puncture resistance. EFDC-.. |
|||
Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | |
BASF HDO® 1,6-Hexanediol Flakes Formula: C6H14O2CAS: 629-11-8Description: 1,6-Hexanediol (HDO) flakes are a colorless, odorless solids or molten masses. It is miscible in water in all proportions and soluble in ethanol.Synonyms: .. |
|||
Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | |
BASF HDO® 1,6-Hexanediol Molten Formula: C6H14O2CAS: 629-11-8Description: 1,6-Hexanediol Molten (HDO) is a colorless, odorless molten mass or solid. It is miscible in water in all proportions and soluble in ethanol.Synonyms: Hexa.. |