Material Notes:
REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are available with a smooth or a unique textured surface that permits pinpoint contact with the load. Sticking can be eliminated as well as providing a surface that breathes, allowing gasses from the ceramic to escape.Applications include firing ceramic capacitors, SOFCs, PZTs, hard and soft ferrites, co-fired substrates and powdered metals. REPTON is available in a wide range of compositions that include a range of alumina, mullite/alumina, zirconia, cordierite, magnesia, and aluminum titanate.
Physical Properties Metric English Comments
Density 6.10 g/cc
0.220 lb/in³
Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Flexural Strength >= 1050 MPa
>= 152000 psi
Thermal Properties Metric English Comments
CTE, linear 9.70 µm/m-°C

@Temperature 300 °C
5.39 µin/in-°F

@Temperature 572 °F
10.3 µm/m-°C

@Temperature 900 °C
5.72 µin/in-°F

@Temperature 1650 °F
Component Elements Properties Metric English Comments
Y2O3 3.0 %
3.0 %
ZrO2 97 %
97 %