Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 2571 Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 2571 Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized under component file E40654. 02571 is available in black or brown color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.590 g/cc
0.0213 lb/in³
ASTM D1895
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Water Absorption 0.32 %
0.32 %
ASTM D570
Linear Mold Shrinkage 0.0079 cm/cm
0.0079 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 88
88
ASTM D785
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Elongation at Break 0.61 %
0.61 %
ASTM D638
Tensile Modulus 8.10 GPa
1170 ksi
ASTM D638
Flexural Strength 76.0 MPa
11000 psi
ASTM D790
Flexural Modulus 7.30 GPa
1060 ksi
ASTM D790
Compressive Strength 209 MPa
30300 psi
ASTM D695
Poissons Ratio 0.36
0.36
ASTM D638
Shear Modulus 2.98 GPa
432 ksi
Calculated
Izod Impact, Notched 0.166 J/cm
0.311 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.195 J/cm²
0.928 ft-lb/in²
ASTM D256
Impact 102
102
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 66.0 µm/m-°C

@Temperature 40.0 - 130 °C
36.7 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 196 °C
385 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 173 °C
343 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 29.1 %
29.1 %
ASTM D2863
Shrinkage 0.27 %
0.27 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 6.50e+11 ohm-cm
6.50e+11 ohm-cm
ASTM D247
Dielectric Constant 4.7
4.7
ASTM D150
Dielectric Strength 12.6 kV/mm
320 kV/in
Short Time; ASTM D149
Dissipation Factor 0.048
0.048
ASTM D150
Arc Resistance 136 sec
136 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved