Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.30 GPa | 1060 ksi | |
Plastcom SLOVAMID 6 GF 15 T 25 LTS PA6, 15% glass fibre, 25% mineral filling FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form /no screw after cooli.. |
|||
Flexural Modulus | 7.30 GPa @Temperature 23.0 °C |
1060 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANAMID 66 A12^ F20 FR6 Nylon 66, Glass Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Modulus | 7.31 GPa | 1060 ksi | 1.3 mm/min; ASTM D790 |
PolyOne Edgetek® PC-30GF/000 BLACK Polycarbonate (PC) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178 |
Nilit FRIANYL B63 H-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178 |
Nilit FRIANYL B63 W-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ASTM D790 |
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Flexural Modulus | 7.31 GPa @Temperature 150 °C |
1060 ksi @Temperature 302 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive. Wear Resistant, Flame Retardant. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific) LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Clean Compounding System, Electrically Conductive, Wear Resistant, Ea.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | 2mm/min; ISO 178 |
Teijin Panlite® GN-3430R Improved Mold Release, Glass Fiber Reinforced, Flame Resistant Polycarbonate Resin GF 30% reinforced, flame retardant and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machin.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | 2mm/min; ISO 178 |
Teijin Panlite® GS-3430 Friction and Abrasion Resistant, Glass Fiber Reinforced Polycarbonate Resin GF 30% reinforced grade, meeting UL 94 V-2. It is compounded with fluorine powder to improve friction and abrasion resistance, maintaining excellent characteristics of polycarbonate resin.Applicatio.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp OK006 PPS - Linear LNP* Thermocomp* OK006 is based on a Linear Polyphenylene Sulfide (PPS) containing Talc.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 7.29 GPa | 1060 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PFW53U PA 6 (Asia Pacific) LNP* THERMOCOMP* PFW53U is a compound based on Nylon 6 resin containing Glass Fiber, Mineral. Added features of this material include: UV Stabilized. |
|||
Flexural Modulus | 7.31 GPa | 1060 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN133TL (Dry) Nylon 66, 33% Glass Fiber Reinforced, Lubricated, Impact Modified Features: Impact modifiedLubricatedGood toughnessForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ASTM D790 |
Plenco 2311 Phenolic, Granular, Injection Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |
|||
Flexural Modulus | 7.31 GPa | 1060 ksi | Tangent; ASTM D790 |
Washington Penn High Modulus Polypropylene Homopolymer 40% Glass Filled Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178-93 |
Wellman Wellamid® GF25-60 XE-NBK1 25% Glass Fiber Reinforced Nylon 6 Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ASTM D790 |
Toyobo Vylopet® EMC310K Glass Reinforced Polyester, Easy Molding Grade Key Feature: HB UL-94 classApplications: General componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemic.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GV 30 HW 30% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO Data |
BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-106A is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The co.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 613 Nylon 6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 223 ABS, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ASTM D790 |
Plenco 7321 Phenolic, Nodular, Compression Molded PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon.. |
|||
Flexural Modulus | 7.30 GPa @Temperature 120 °C |
1060 ksi @Temperature 248 °F |
ISO 178 |
DSM Stanyl® TS200F10 PA46-GF50 50% Glass Reinforced |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | conditioned, 2 mm/min; ISO 178-A |
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |