Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.30 GPa | 1060 ksi | |
Plastcom SLOVAMID 6 GF 15 T 25 LTS PA6, 15% glass fibre, 25% mineral filling FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form /no screw after cooli.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | |
Plastcom SLOVAMID 6 GF 15 T 25 TS PA6, 15% glass fibre, 25% mineral filling FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form /no screw after cooli.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178 |
Nilit FRIANYL B63 H-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178 |
Grupo Repol Dinalon® A1S25 G35 H PA66 35% Glass Fiber, Heat Stabilized Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178 |
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ASTM D790 |
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP IFL36R PA6.12 (Europe-Africa-Middle East) Internally lubricated PA6.12, containing Glass Fiber and PTFE |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive. Wear Resistant, Flame Retardant. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold .. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC (Asia Pacific) LNP* Stat-kon* DX05474 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Ret.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | 2mm/min; ISO 178 |
Teijin Panlite® GS-3430 Friction and Abrasion Resistant, Glass Fiber Reinforced Polycarbonate Resin GF 30% reinforced grade, meeting UL 94 V-2. It is compounded with fluorine powder to improve friction and abrasion resistance, maintaining excellent characteristics of polycarbonate resin.Applicatio.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp OK006 PPS - Linear LNP* Thermocomp* OK006 is based on a Linear Polyphenylene Sulfide (PPS) containing Talc.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MC004 PP (Europe-Africa-Middle East) LNP* Thermocomp* MC004 is a compound based on Polypropylene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ASTM D790 |
Plenco 2571 Phenolic, Granular, Transfer Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178-93 |
Wellman Wellamid® GF25-60 XE-NBK1 25% Glass Fiber Reinforced Nylon 6 Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178 |
Polyram RamLloy PN300G6 PPE/PS Alloy, 30% Glass Fiber PPE/PS alloy, 30% glass fiber reinforced for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ASTM D790 |
Toyobo Vylopet® EMC310K Glass Reinforced Polyester, Easy Molding Grade Key Feature: HB UL-94 classApplications: General componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemic.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178 |
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/HK060AE Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GV 30 HW 30% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO Data |
BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-106A is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The co.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 223 ABS, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ASTM D790 |
E-Polymers Tekaloy® G70GFR , Flame Retardant, 30% Glass Fiber Reinforced PC/ABS Alloy 30% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC (Asia Pacific) LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Flexural Modulus | 7.30 GPa | 1060 ksi | ASTM D790 |
Plenco 7321 Phenolic, Nodular, Compression Molded PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon.. |
|||
Flexural Modulus | 7.30 GPa @Temperature 120 °C |
1060 ksi @Temperature 248 °F |
ISO 178 |
DSM Stanyl® TS200F10 PA46-GF50 50% Glass Reinforced |