Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6.50e+11 ohm-cm | 6.50e+11 ohm-cm | JIS-K-6249/ASTM D257 |
Fujipoly Industries Sarcon® GR-Hn Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Volume Resistivity | 6.50e+11 ohm-cm | 6.50e+11 ohm-cm | ASTM D247 |
Plenco 2571 Phenolic, Granular, Transfer Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |