Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
Plaskolite Optix® CA-927 Impact Modified Acrylic Resin Injection Molding Grade Pellets. Better impact strength than CA-924. Excellent surface gloss, optical clarity, and practical toughness. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
Plaskolite West Optix® CA-927 Impact Modified Acrylic Resin Injection Molding Grade Pellets. Better impact strength than CA-924. Excellent surface gloss, optical clarity, and practical toughness. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral filled PA6 non-halogen FR compound |
|||
Flexural Strength | 76.0 MPa | 11000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
Eastman Eastalloy DA510 Polymer
(discontinued **) Eastalloy Polymer DA510 is a clear copolyester/polycarbonate alloy. This product has good physical properties. These include good impact strength, chemical resistance, heat resistance, dimensional s.. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
Ineos Nova 2504 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Good balance of flow, strength and heat resistance, USP Class VI Applications: Consumer electronics, HousewaresExposure to gamma radiation in the 2.02-6.06 megarad range has no .. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
Kolon KOCETAL® VT301 Anti-Static Grade Acetal Resin Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
Kolon KOCETAL® WR301 Wear Modified Acetal Resin Improved weather resistant grade suitable for out door use. Applications: Weather resistant products. Information provided by API-Kolon. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12 LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KP004AXC Acetal Homopolymer LNP LUBRICOMP* KP004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA 6/10 (Asia Pacific) LNP* Lubricomp* QAP22S is a compound based on Nylon 6/10 resin containing PTFE, Aramid Fiber, Silicone. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA6.10 LNP* LUBRICOMP* QAP22S is a compound based on Nylon 6/10 resin containing 10% PTFE/Silicone, 10% Aramid Fiber. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | at rupture; ASTM D790 |
Sumitomo Bakelite North America EM 7400-2 Long Glass Fiber Reinforced Epoxy EM 7400-2 is a polyaramide fiber reinforced epoxy molding compound, which features abrasion resistance and light weight.Information provided by Sumitomo Bak North America, Inc. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MX89510 PP LNP* THERMOCOMP* MX89510 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Flexural Strength | 76.0 MPa | 11000 psi | |
Sumitomo Bakelite Durez® 25378 Phenolic, Injection Grade Durez 25378 Black Phenolic is a two stage heat resistant/electrical grade molding material having an excellent molded finish, low shrinkage and good heat resistance. Durez 25378 has exceptional UL .. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
Plenco 2571 Phenolic, Granular, Transfer Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | |
Cosmic Plastics ID-50 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
Plenco 4300 Phenolic, Granular, Compression Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ISO 178 |
Polyplastics Duracon® WR-01 Acetal Co-polymer (POM), Chlorine water resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
Videolar 500 Crystal Polystyrene (GPPS) Designed for injection moldingVery easy flowing grade for fast cycle injection moldingExcellent processability for filling thin partsFeatures: Good strengthGood temperature resistanceExcellent clari.. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | |
Cosmic Plastics D45 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ISO 178 |
Denka MALECCA K-095 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
Diamond Polymers NYLON 6630 L Black Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | 2 mm/min; ISO 178 |
Chi Mei Polyrex® PG-80N Polystyrene High strength |
|||
Flexural Strength | 76.0 MPa @Temperature 120 °C |
11000 psi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry) Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla.. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ISO 178 |
BASF Ultradur® B 6550 LN PBT Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
SABIC Innovative Plastics NORYL PX2630 PPE+HIPS (Asia Pacific) PPE+HIPS Unfilled high Impact |
|||
Flexural Strength | 76.0 MPa | 11000 psi | 2 mm/min; ISO 178 |
Sax Polymers SAXALEN PPC343G20 Polypropylene Copolymer, 20% Glass Filled SAXALEN PPC343G20 is a 20% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |
|||
Flexural Strength | 76.0 MPa | 11000 psi | |
Cosmic Plastics 6160 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | |
Cosmic Plastics D44 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |