Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastics Group Polifil® GFPC-30 30% Glass-Reinforced Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 30% Glass Filled
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® GFPC-30 30% Glass-Reinforced Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycarbonate line an excellent choice for electrical, appliance and hardware applications. Standard processing techniques are applicable. Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Filler Content 30 %
30 %
ASTM D2584
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm

@Thickness 1.59 mm
0.0020 - 0.0030 in/in

@Thickness 0.0625 in
ASTM D955
Melt Flow 12 - 20 g/10 min
12 - 20 g/10 min
300/1.2; May be specified; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 92
92
ASTM D785
Tensile Strength at Break 130 MPa
18800 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Tensile Modulus 8.62 GPa
1250 ksi
ASTM D790
Flexural Strength 157 MPa
22700 psi
ASTM D790
Flexural Modulus 7.93 GPa
1150 ksi
Tangent; ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
At 73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
295 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved