Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Hexion Bakelite™ X24 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled.Application areas: Operating controls, housing parts, lamp holders.Information provided by Bak AGBak AG became a part of Hexion in 2005. |
|||
Density | 1.43 - 1.47 g/cc | 0.0517 - 0.0531 lb/in³ | ISO R 1184 |
Fainplast Compounds RH 210/K1 Rigid PVC, Antishock Extrusion Antishock profiles |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | 9743A |
Lord Adhesives Aeroglaze® 9743 Epoxy Primer/Tie-Coat Aeroglaze® 9743 is a two-part epoxy primer designed for use on aluminum, metal, and prepared composite surfaces. Aeroglaze 9743 primer/tie-coat can be applied to scuff-sanded urethane top coats a.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | |
LATI Laticonther 52/11 CP3/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP002 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP LCL33E PEEK LNP LUBRICOMP* LCL33E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Easy Molding, Wear Resistant. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 (Asia Pacific) LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES HiFill® PET GF15 X BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA6/6 GF30 ML5 HS 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(5%)Features: Lubricated and Heat Stabiliz.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp EB004 PEI LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP EC008PXQ PEI LNP* THERMOCOMP* EC008PXQ is a compound based on Polyetherimide containing 40% Carbon FIber. Added features include: Electrically Conductive, Exceptional Processing |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp LC008 PEEK (Europe-Africa-Middle East) LNP* Thermocomp* LC008 is a compound based on Polyetheretherketone resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
PlastxWorld CEVIAN® B6524 20% GF PBT/ABS Alloy Glass fiber and mineral filled, low warpage and flame retarded PBT/ABS.Information provided by PlastxWorld Inc. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Plenco 2369 Phenolic, Granular, Compression Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Polyplastics Duranex® 2016 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50% DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Tisan TISESTER® Flame Retardant (V0). Heat Stabilized Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Chengdu Polyster FH5550 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H5550 and self-made flame retardant material. Flame retardant, good balance of low and high temperature properties. Applications requiring flame retardancy, such as wires, cables and optica.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | dry; ISO 1183 |
DSM Stanyl® TS350 PA46 FR(17) Unreinforced, Flame Retardant |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | DAM; ISO 1183 |
DSM Stanyl® TW275F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified (Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792, ISO 1183 |
EPICHEM Epinyl PA 66 GF25 AU Polyamide 66, 25% Glass, Self extinguishing Characteristics: 25% glass fibre filled |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D1505 |
DuPont Teijin Films Melinex® 329 Polyester Film, 300 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D1505 |
DuPont Teijin Films Melinex® 331W Polyester Film, 200 Gauge An opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings. 331W has same properties as 331 with the only ex.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Density | 1.43 - 1.47 g/cc | 0.0517 - 0.0531 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HF 045/16M Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, low shrinkageInformation provided by Fainplast Compounds |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | |
Bond Laminates TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate Within the TEPEX® composite laminate, Polyamide 66 is a resin known for its high hardness, stiffness, abrasion resistance, heat and chemical resistances. The carbon used within this material is ae.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | Liquid |
3M Novec™ 8200 Engineered Fluid 3M™ Novec™ 8200 Engineered Fluid is a clear, colorless, low-odor fluid intended to replace 1,1,1-trichloroethane and perchloroethylene in film cleaning applications.Features and Benefits:Zero ozon.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D1505 |
DuPont Teijin Films Melinex® 339 Polyester Film, 200 Gauge Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339.. |