Petromont 4100 High Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Petromont
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petromont 4100 High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Petromont HDPE 4100 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for general use in large diameter heavy duty and non pressure pipe applications. The applications include profile and corrugated pipes, sewers, culverts and communication conduits.Petromont HDPE 4100 is a high molecular weight hexene modified resin with a broad molecular weight distribution offering excellent extrusion characteristics and processability, combined with an excellent toughness and excellent stress cracking resistance. This grade’s material classification is PE345440A according to the standard ASTM D 3350-02a, according to D 3350-05, it became PE445440A. It is not a pressure rated resin.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 2000 hour
>= 2000 hour
F<sub>50</sub>; ASTM D1693-B
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
F<sub>50</sub>; ASTM D1693-B
Melt Flow 0.10 g/10 min
0.10 g/10 min
I<sub>2</sub>; ASTM D1238
10 g/10 min
10 g/10 min
I<sub>21</sub>; ASTM D238
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.5 MPa
5000 psi
ASTM D638
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
ASTM D790
Izod Impact, Notched >= 2.13 J/cm
>= 3.99 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Process Pipe Extrusion